Working Power: AC220V 50Hz/60Hz Gross Weight: 49kg
DSC Range: 0 ~ ± 500mW Temperature Accuracy: ± 0.1 ° C
Display Mode: 24bit Color, 7 Inch LED Touch Screen Display DSC Noise: 0.001mW
DSC Sensitivity: 0.001mW
Highlight:

600C DSC Calorimeter

,

0.001mW Differential Scanning Calorimeter

,

AC220V DSC Calorimeter


Product Description

BAXIT DSC 600C differential scanning calorimetry price

 

 

Overview:

Differential Scanning Calorimetry (DSC) is a classical thermal analysis method for the thermal effect of programmable temperature. It is used in various research and development, process optimization, quality control and failure analysis in various materials and chemistry fields. Occasionally, it has been widely used. Using the DSC method, we can study the phase transition of inorganic materials, the melting of polymer materials, the crystallization process, the polymorphism of drugs, and the solid/liquid phase ratio of foods such as oils and fats. In line with national standard GB/T2951.42-2008, GB/T15065-2009, GB/T17391-1998, GB/T19466.6-2009.

Technical characteristics:

1, industrial-grade wide-screen touch structure, display information is rich, including set temperature, sample temperature, oxygen flow, nitrogen flow, differential heat signal, various switch states.

2. New designed oven structure ensures high resolution and good stability of base line;
3. Air flow meter may control the air flow rate accurately; the test data can be recorded into the database directly;
4. The instrument is bilateral control, may be controlled by both main frame and software. User-friendly interface, easy operation.

5, dual temperature probe to ensure high repeatability of sample temperature measurement.

6. The digital gas mass flow meter automatically switches the two-way air flow, and the switching speed is fast and the stabilization time is short.

7. Standard samples are standard to facilitate the customer to correct the temperature coefficient.

8, software adaptive resolution computer screen; support notebook, desktop, support WIN2000, XP, WIN7, WIN8, WIN10 and other operating systems.

9. Support user self-programming program to realize full automation of measurement steps. The software provides dozens of instructions, and the user can flexibly combine the instructions according to their own measurement steps and save them. Complex operations are simplified into one-button operation.

Technical Parameters:

DSC range 0 ~ ± 500mW
Temperature range room temperature ~ 600 ° C
Heating rate 0.1~80°C/min
Temperature resolution 0.01 ° C
Temperature accuracy ± 0.1 ° C
Temperature repeatability ± 0.1 ° C
DSC accuracy ± 2%
DSC resolution 0.001mW
DSC sensitivity 0.001mW
Temperature control mode Heating, constant temperature, cooling, cycle temperature control (full program automatic control)
Curve scan Temperature scan
Atmosphere control Gas mass flow meter automatically switches two gas channels
Display mode 24bit color, 7 inch LED touch screen display
Data interface USB standard interface, supporting the corresponding operating software
Parameter standard Equipped with standard calibrator with one-button calibration function, users can calibrate the temperature by themselves
Working power AC220V 50Hz/60Hz

 

Applications:

Measure physical and chemical changes related to heat, such as glass transition temperature and melting point. Melting temperature, crystallization and crystallization heat, phase transition heat, product thermal stability, solidification/crosslinking, oxidation induction period, reaction kinetics, specific heat, and the like.